Volume variation in filled and unfilled natural rubber : competition between cavitation and stress-induced crystallization

this is a study on the competition between cavitation and stress-induced crystallization during the deformation of cis-1,4 polyisoprene rubber. During deformation, this kind of material exhibits volume variation induced by both phenomena. In this study, we propose to measure this volume variation by an original full-field measurement technique. The high resolution of this technique allows us to identify characteristic stretch ratios during mechanical cycles.