probe tack test

LECAM's picture

Experimental analysis of prepreg tack

Dear all, I post a study dealing with tack of prepreg materials. This kind of composite materials is increasingly used in the design of structural parts, particularly in the aerospace industry.Tack is one of the major properties that governs the ability of prepreg to be laid up. To investigate this property, we have developed a probe tack test to evaluate the effect of the temperature, the contact time, the contact force and the debonding rate on it.