Spatial Control in the Heterogeneous Nucleation of Water

The attache d paper was recently published
in Applied Physics Letters. We show for the first time that Nucleation and
Condensation of Water can be spatially controlled. Such control of nucleation
phenomena and the fundamental findings discussed in the paper have implications
for the Energy and Water industry. The paper can be found at http://link.aip.org/link/?APL/95/094101/1

Kripa Varanasi's picture

Spatial Control in the Heterogeneous Nucleation of Water

The attached paper was recently
published in Applied Physics Letters. We show for the first time that
Nucleation and Condensation of Water can be spatially controlled. Such control
of nucleation phenomena and the fundamental findings discussed in the paper have
implications for the Energy and Water industry.

The paper can be found at
http://link.aip.org/link/?APL/95/094101/1

Subscribe to RSS - superhydrophilic

Recent comments

More comments

Syndicate

Subscribe to Syndicate