Skip to main content

structural models for carbon nanotubes

Breakdown of structural models for zigzag single wall carbon nanotubes

Submitted by rbatra on

The following article shows that the linear elasticity theory does
not predict well inextensional modes of vibration of a single-wall
zig-zag tube.

 Gupta, S.S., Bosco, F.  and 
Batra, R. C. (2009) Breakdown of structural models for vibrations of
single-wall zigzag carbon nanotubes, J.
Applied Physics,
106,
063527.