Skip to main content

wear testing

Special Tutorial during WOM 2013: Fundamentals of Wear and Wear Testing

Submitted by Laure Ballu on

Taught by invited experts led by Professor Ian Hutchings, this popular half-day overview will be held on Sunday afternoon before the WOM 2013 conference Portland, Oregon, 14-18 April 2013.

The content is intended to help delegates who are new to the subject, or would like to refresh their background knowledge, and the lecturers aim to cover the general principles of wear and tribological testing. Printed notes will be provided for delegates.

The course outline includes:

Coefficient of Friction & Wear Testing of Plasma Coating

Submitted by NANOVEA on

A major concern for plasma coatings is how wear resistant they will prove to be on the final product. Since

plasma coatings are a popular use for automobile engines, these coatings are tested through strenuous

conditions. If the coating on the engine itself wears off at a fast rate than the life expectancy of that

particular engine or part becomes a problematic concern. With the plasma coating wearing off, the parts

originally being protected will become exposed to melting temperatures, corrosion and other potentially