Reversible nanopore formation in Ge nanowires during lithiation-delithiation cycling: an in situ TEM study Submitted by Jianyu Huang on Tue, 08/23/2011 - 00:14 research lithium ion battery in situ TEM Germanium nanowire sponge pore memory effect (PME) reversible volume change Nano Lett. 2011, DOI: 10.1021/nl2024118 Read more about Reversible nanopore formation in Ge nanowires during lithiation-delithiation cycling: an in situ TEM studyLog in to post comments5047 views