photonic gel

Modeling mechano-chromatic lamellar gels

Submitted by Wei Hong on

Consisting of alternating swelling and nonswelling polymeric layers (SLs and NLs), lamellar gels are 1D photonic crystals with tunable optical properties.  The lamellar structure induces a constraint between the SLs and the NLs, resulting in an anisotropic swelling behavior coupled with deformation.