A molecular dynamics study of the thermal conductivity of nanoporous silica aerogel, obtained through negative pressure rupturin Submitted by Jingjie Yeo on Mon, 04/02/2012 - 03:38 research Silica aerogel Reverse non-equilibrium molecular dynamics Negative pressure rupturing Thermal conductivity http://dx.doi.org/10.1016/j.jnoncrysol.2012.03.007 Read more about A molecular dynamics study of the thermal conductivity of nanoporous silica aerogel, obtained through negative pressure rupturinLog in to post comments4307 views