Polymer constitutive modelling: Formulation and computational aspects

Submitted by Mirkhalaf on
  • This work formulates an elasto-viscoplastic model at finite strains.
  • A particularly efficient numerical integration algorithm is presented.
  • A closed-form analytical expression is derived for the consistent tangent operator.
  • The non-linear behaviour of polymers is captured in the numerical examples.
  • Quadratic rate of convergence is successfully achieved.

doi:10.1016/j.compstruc.2016.01.002

 

Position is not anymore available --- Research Position at TU Darmstadt

Submitted by xubaixiang on


At the Division of Mechanics
of Functional Materials in the institute of Materials Science, TU Darmstadt the
following research position is to be filled as soon as possible:

 Research position (E 13 TV โ€“ TU
Darmstadt),
Doctoral Candidate/Postdoc

The position is first
scheduled for three years in the case of doctoral candidate and two years in
the case of Postdoc (an extension is possible).

 

Tasks and Opportunities