Review of a few "Unified" Viscoplasticity Models (Motivated by solder deformation)

I had prepared this document for a class project, the level is introductory and the selection of models is motivated by solder deformation, but I hope it is of some help. I have examined four models, proposed by Hart, Anand, Krempl and Busso. The document has 16 pages.