Local water slamming impact on sandwich composite hulls
Recently we analyzed water-slamming impacts on sandwich composite hulls. Water slamming impact problems are very interesting problems involving fluid-structure interactions. A link to our paper and the abstract are given below. I hope that you will find the paper interesting. Please feel free to write your comments below.
Kaushik Das and Romesh C. Batra, Local water slamming impact on sandwich composite hulls, Journal of Fluids and Structures, Volume 27, Issue 4, May 2011, Pages 523-551