Mesoscale Constitutive Modeling of Non-Crystallizing Filled Elastomer
We have just published a new paper, 1st in the series, that presents a computational model to understand the microstructural changes in the filled elastomers as a consequence of mechanical forces. A heterogeneous (or multiphase) constitutive model at the mesoscale explicitly considering filler particle aggregates, elastomeric matrix and their mechanical interaction through an approximate interface layer is presented. An innovative lego-set method is discussed for generation of random microstructures that can be used for simple stochastic analysis.