Submitted by shanmugam39510 on Tue, 10/16/2012 - 05:20 i'm analysing the rc beam by using ansys APDL software span = 2000mm cross section = 150 x 300 mm my question is HOW TO MESH THE CONCRETE VOLUME AND REINFORCEMENT (BOTH) Forums iMechanica Get Together Forum software Free Tags RC beam eng.rj hi, i suggest you to draw hi, i suggest you to draw small concrete element (solid65) , then copy it to make the beam then you draw one reinforcement elemant ( link8) between two concrete nodes , then copy it good luck Log in or register to post comments Sat, 10/27/2012 - 22:12 Permalink Log in or register to post comments5202 views
eng.rj hi, i suggest you to draw hi, i suggest you to draw small concrete element (solid65) , then copy it to make the beam then you draw one reinforcement elemant ( link8) between two concrete nodes , then copy it good luck Log in or register to post comments Sat, 10/27/2012 - 22:12 Permalink
hi, i suggest you to draw
hi,
i suggest you to draw small concrete element (solid65) , then copy it to make the beam
then you draw one reinforcement elemant ( link8) between two concrete nodes , then copy it
good luck