Super stretchy carbon nanotubes
Huang et al., PRL 98, 185501 (2007)
Watch movies at: http://netserver.aip.org/cgi-bin/epaps?ID=E-PRLTAO-98-002719
We report exceptional ductile behavior in individual double-walled and triple-walled carbon nanotubes at temperatures above 2000 C, with tensile elongation of 190% and diameter reduction of 90%, during in situ tensile-loading experiments conducted inside a high-resolution transmission electron microscope. Concurrent atomic-scale microstructure observations reveal that the superelongation is attributed to a high temperature creep deformation mechanism mediated by atom or vacancy diffusion, dislocation climb, and kink motion at high temperatures. The superelongation in double-walled and triple-walled carbon nanotubes, the creep deformation mechanism, and dislocation climb in carbon nanotubes are reported here for the first time.
Attachment | Size |
---|---|
![]() | 2.04 MB |
- Jianyu Huang's blog
- Log in or register to post comments
- 9406 reads

Comments
Excellent work!
Excellent! I really like this paper. Could you please post your paper to the J-Club May 2007 issue? I believe that your paper will attract huge attention and help stimulate discussion for the J-Club May 2007 issue.
Thanks a lot for your comment!
Prof.Li, I already posted my paper in the J-Club.
Super!!
Fabulous work done!!
Thank you very much!
I appreciate it!!!
Great
Great but it would be wonderful if we could model it using Mollecular Dynamics Simulation, and we could find out more details on its cause.