Submitted by ashfaqadnan on Thu, 08/23/2007 - 19:16 mechanical properties Single Crystal lattice parameters Hi, I truly appriciate if anyone can help me find mechanical properties and crystal structure of beta SiC single crystals. Any reference or link will be highly appriciated Sincerely, -Ashfaq Adnan ashfaqadnan Single Crystal, Mechanical Properties, Lattice Parameters Ashfaq Adnan Phd Student, Schoold of Aeronautics and Astronautics Purdue University, West Lafayette, Indiana 47907 Log in or register to post comments Thu, 08/23/2007 - 19:16 Permalink Xiaodong Li Re: Single Crystal, Mechanical Properties, Lattice Parameters You can find the mechanical properties of SiC films from the paper below. Hope this helps. Xiaodong Li and Bharat Bhushan, "Micro/Nanomechanical Characterization of Ceramic Films for Microdevices," Thin Solid Films, 340 (1999) 210-217. Log in or register to post comments Fri, 08/24/2007 - 00:32 Permalink Log in or register to post comments8358 views
ashfaqadnan Single Crystal, Mechanical Properties, Lattice Parameters Ashfaq Adnan Phd Student, Schoold of Aeronautics and Astronautics Purdue University, West Lafayette, Indiana 47907 Log in or register to post comments Thu, 08/23/2007 - 19:16 Permalink
Xiaodong Li Re: Single Crystal, Mechanical Properties, Lattice Parameters You can find the mechanical properties of SiC films from the paper below. Hope this helps. Xiaodong Li and Bharat Bhushan, "Micro/Nanomechanical Characterization of Ceramic Films for Microdevices," Thin Solid Films, 340 (1999) 210-217. Log in or register to post comments Fri, 08/24/2007 - 00:32 Permalink
Single Crystal, Mechanical Properties, Lattice Parameters
Ashfaq Adnan
Phd Student, Schoold of Aeronautics and Astronautics
Purdue University, West Lafayette, Indiana 47907
Re: Single Crystal, Mechanical Properties, Lattice Parameters
You can find the mechanical properties of SiC films from the paper below. Hope this helps.
Xiaodong Li and Bharat Bhushan, "Micro/Nanomechanical Characterization of Ceramic Films for Microdevices," Thin Solid Films, 340 (1999) 210-217.