Hi,
I am working on Epoxy material damage for a research project. We observed from the experiments that the Epoxy material just fails without any plastic deformation and tensile yield strength is lower than compression (2-3 times). So, inorder to simulate the material damage model in Abaqus, could anyone advise me that which damage model I should consider for my analysis?. Most of the material-damage models available for ductile materials, for example, General Ductile, Jhonson-Crook, Druckker Prager model, atc..Although I could see brittle cracking mode, its only availble in Abaqus/Explicit if am not wrong..
Thanks in advance,,
Bernad
- bernad's blog
- Log in or register to post comments
- 5458 reads
Comments
you should have a look at
you should have a look at abaqus Czone plugin