Hi. I'm working on multiscale modeling of soft tissues. I'm working
on modeling an orthotropic wavy fiber in WB. I write an APDL routine to
change the element coordinate system of each element with accordance to
the fiber curvature. Ansys documentation said that in the case of large
deflection analysis, the element coordinate system will be rotated with
accordance to element rigid body rotation. My problem is that, after the
solution, the elements coordinate system of some elements rotate
more/less than the rigid body rotation of the elements and fiber
curvature. I'm wondering if any body can help me with this problem