Submitted by Parag Tandaiya on Tue, 02/20/2024 - 15:25 research Bulk Metallic Glasses Dynamic Compression Finite Element simulations Constitutive model SHPB setup high strain rate Elevated temperatures I would like to share our following paper published recently in International Journal of Plasticity: Modeling and simulation of dynamic compression of Bulk Metallic Glasses at room and elevated temperatures using split Hopkinson pressure bar setup Log in to post comments2119 views