Elastic response of mesoporous silicon to capillary pressures in the pores upon water condensation Submitted by hanjob on Tue, 07/07/2015 - 08:07 research elasticitiy pore-load modulus Nanoporous Materials mesoporous materials capillary effect nano-structured materials; nanocrystalline silicon FEM Deformation characterization; Microscale deformation; SEM Study on the elastic response (macroscopic deformation) of mesoporous silicon upon capillary condensation of water in the pores published in Applied Physics Letters (APL 106, 261901 (2015)). Read more about Elastic response of mesoporous silicon to capillary pressures in the pores upon water condensationLog in to post comments2367 views