Finite strain mean-field homogenization of composite materials with hyperelastic-plastic constituents Submitted by Marieme Imene … on Wed, 07/13/2016 - 12:45 research Plasticity finite strain composite materials Elastic-plastic material Abstract: Read more about Finite strain mean-field homogenization of composite materials with hyperelastic-plastic constituents1 commentLog in to post comments6154 views