tungsten

Uniaxial deformation of tungsten nanopillars/nanowires/nanotubes: Atomistic and coarse-grained atomistic simulations

Submitted by Shuozhi Xu on

Dear Colleague,

In the last two years, we published six papers on uniaxial deformation of tungsten nanopillars/nanowires/nanotubes using atomistic and coarse-grained atomistic simulations: