Through-the-thickness stress

On laminated structures under flexure

Submitted by Lorenzo Bardella on

If you design laminated structures, such as sandwich panels, you might be interested in knowing that the through-the-thickness normal stress, properly disregarded in homogeneous structures, may play a fundamental role in triggering delamination.