buckling

Buckling behavior of metal film/substrate structure under pure bending

Submitted by Ying Li on

Many studies on the thin film/substrate structure and its failure mechanism were reported in recent years. The direct experimental results of thin film/substrate structure by scanning electron microscopy (SEM) presents an intriguing problem:there exists a buckling failure mechanism at the lateral edge of metal film under pure bending. The qualitative theoretical analysis has been done on such buckling failure of thin film/substrate structure.

Fabrication and Characterization of Patterned Single-Crystal Silicon Nanolines

Submitted by Minkyoo Kang on


B. Li, M. K. Kang, K. Lu, R. Huang, P. S. Ho, R. A. Allen, and M. W. Cresswell, Nano Letters 8, 92 -98 (2008).
(Web Release Date: 07-Dec-2007; DOI: 10.1021/nl072144i)

 

Thin films: wrinkling vs buckle-delamination

Submitted by Rui Huang on

H. Mei, J.Y. Chung, H.-H. Yu, C.M. Stafford, and R. Huang, Buckling modes of elastic thin films on elastic substrates. Applied Physics Letters 90, 151902 (2007).

Two modes of thin film buckling are commonly observed, one with interface delamination (e.g., telephone cord blisters) and the other with no delamination (i.e., wrinkling). Which one would occur for your film?

Dynamics of wrinkle growth and coarsening in stressed thin films

Submitted by Sehyuk Im on

Rui Huang and Se Hyuk Im, Physical Review E 74, 026214 (2006).

A stressed thin film on a soft substrate can develop complex wrinkle patterns. The onset of wrinkling and initial growth is well described by a linear perturbation analysis, and the equilibrium wrinkles can be analyzed using an energy approach. In between, the wrinkle pattern undergoes a coarsening process with a peculiar dynamics. By using a proper scaling and two-dimensional numerical simulations, this paper develops a quantitative understanding of the wrinkling dynamics from initial growth through coarsening till equilibrium. It is found that, during the initial growth, a stress-dependent wavelength is selected and the wrinkle amplitude grows exponentially over time. During coarsening, both the wrinkle wavelength and amplitude increases, following a simple scaling law under uniaxial compression. Slightly different dynamics is observed under equi-biaxial stresses, which starts with a faster coarsening rate before asymptotically approaching the same scaling under uniaxial stresses. At equilibrium, a parallel stripe pattern is obtained under uniaxial stresses and a labyrinth pattern under equi-biaxial stresses. Both have the same wavelength, independent of the initial stress. On the other hand, the wrinkle amplitude depends on the initial stress state, which is higher under an equi-biaxial stress than that under a uniaxial stress of the same magnitude.

Surface effects on thin film wrinkling

Submitted by Rui Huang on

A recent discussion here about the effect of surface stress on vibrations of microcantilever has gained some interest from our members. A few years ago, Zhigang and I looked at surface effect on buckling of a thin elastic film on a viscous layer (Huang and Suo, Thin Solid Films 429, 273-281, 2003). Although the physical phenomena (buckling vs vibrations) are different, the conclusion is quite consistent with Wei Hong and Pradeep's comments toward the end of the discussion. That is, surface stress only contributes as a residual stress and thus does not affect the buckling wavelength (frequency in space in analogy to frequency in time for vibrations).

Why fingerprints are different

Submitted by Konstantin Volokh on

A possible explanation of the variety of fingerprints comes from the consideration of the mechanics of tissue growth. Formation of fingerprints can be a result of the surface buckling of the growing skin. Remarkably, the surface bifurcation enjoys infinite multiplicity. The latter can be a reason for the variety of fingerprints. Tissue morphogenesis with the surface buckling mechanism and the growth theory underlying this mechanism are presented in the attached notes.