bone microstructure

Yield behaviour of trabecular bone

Submitted by Lee Margetts on

A recently published paper  "Evaluating the macroscopic yield behaviour of trabecular bone using a nonlinear homogenisation approach" links the micromechanics of bone to its macroscopic behaviour. The paper may be of interest to colleagues on this forum. The abstract is provided below.

Abstract: