Cyclic volume changes in rubber

This is a study dealing with the volume variation in filled crystallizable natural (F-NR) and uncrystallizable styrene butadiene (F-SBR) rubbers subjected to cyclic loadings. During their deformation, such materials exhibit volume variation induced by the cavitation phenomenon and the decohesion between particles and the rubber matrix.