Disparity in Simple Shear solution in ABAQUS
Forums
Choose a channel featured in the header of iMechanica
Free Tags
Dear All,
We tried to simulate simple shear using ABAQUS and compared it with the analytical solution. To our surprise, even though the equivalent stress and strain matched perfectly, the component stress and strain had a large deviation between the semi analytical and ABAQUS methods. The zero components in the analytical model were calculated to be non-zero in the results of ABAQUS. This paradox could not be understood clearly as whether it is a case of software deficiency or conceptual error. A COMPLETE ANALYSIS OF THE PROBLEM IS ATTACHED AS A REPORT.