Tunable Tail Swing of Nanomillipedes

Submitted by Fan Xu on

The physical properties of graphene nanoribbons (GNRs) are closely related to their morphology; meanwhile GNRs can easily slide on surfaces (e.g., superlubricity), which may largely affect the configuration and hence the properties. However, the morphological evolution of GNRs during sliding remain elusive. We explore the intriguing tail swing behavior of GNRs under various sliding configurations on Au substrate. Two distinct modes of tail swing emerge, characterized by regular and irregular swings, depending on the GNR width and initial position relative to the substrate.