Composite Manufacturing Process Modeling Using Poromechanics

Modeling and simulation of manufacturing of advanced composite material is a must in today's industry as the use of advance composites is increasing dramatically. The aim is to reduce the number of trial and error by development of a simulation tool to model and predict the manufacturing fundamental phenomena happening simultaneously in different scales. Poromechanics is a multidisciplinary and multiphysics concept which can be used to achieve this goal.