High-Performance Multiresponsive Paper Actuators Submitted by mortezaamjadi on Wed, 10/19/2016 - 11:47 research actuators electromechanical actuators hygro-mechanics Silver nanowire soft robotics Published in ACS Nano: http://pubs.acs.org/doi/abs/10.1021/acsnano.6b05545 Read more about High-Performance Multiresponsive Paper ActuatorsLog in to post comments3255 views