Calculation of coefficient of thermal expansion of graphene using MD simulations with various thermostats Submitted by Nuwan Dewapriya on Fri, 08/16/2013 - 16:31 research molecular dynamics graphene Berendsen Thermostat CTE equilibrium Nose-Hoover Langevin Read more about Calculation of coefficient of thermal expansion of graphene using MD simulations with various thermostatsLog in to post comments6596 views