Nanoscale Mechanics of the Solid Electrolyte Interphase on Lithiated-Silicon Electrodes
Hello Imechanica community, we have just published our study on the mechanics of SEI in Li-ion batteries. Please find the abstract and link as below.
Abstract:
Abstract: