Case Study Effect of Pore Size on Pellet-Based Catalyst Flow

Submitted by Simpleware on

We have a new case study on our website based on research at Imperial College into multiscale tomography and calculating permeability for catalysts. The project involved studying the influence of pore structure on fluid flow across large length scales in silica-alumina pellet-based catalysts.

3D data at different length scales was obtained from XMT, DBFIB-SEM and ET scanning and segmented into a binarised dataset.