Elastic Bounds of Bioinspired Nanocomposites
Biological materials in nature serve as a valuable source of inspiration for developing
novel synthetic materials with extraordinary properties or functions. Much effort to date
has been directed toward fabricating and understanding bio-inspired nanocomposites
with internal architectures mimicking those of nacre and collagen fibril. Here we establish
simple and explicit analytical solutions for both upper and lower bounds of the elastic