Spiral fracture in metallic glasses and its correlation with failure criterion
Xianqi Lei,Yujie Wei, Bingchen Wei, Wei-Hua Wang. Acta Materialia 99, 206-212 (2015). doi:10.1016/j.actamat.2015.08.008
Wellcome comments and suggestions!
Mechanical research engineer in Fatigue Analysis of 304L Steel
Context :
EDF Research and Development and EDF Energy are currently developing their new centre: the EDF Energy R&D UK Centre. In addition, EDF R&D and the University of Manchester have created the Modelling and Simulation Centre in 2011. In the scope of the development of nuclear energy in the UK, EDF R&D and EDF Energy Generation wish to take advantage of this new centre in Manchester.
Topic :
Special Issue Announcement in CMAME on 'Phase Field Approaches to Fracture'
Dear Colleagues,
Strengthening high-stacking-fault-energy metals via parallelogram nanotwins
A variety of questions remain open in the new form of nanotwins in Ni, welcome any comments!
Visiting Scientist Program at University of Cagliari
The University of Cagliari has launched the Visiting Scientists Programme.
The deadline for application is 10/09/2015
http://people.unica.it/researchersinmotion/visiting-scientist-2/
Position and salary grade is set for leading scientists.
Contact: Prof. Michele Brun
http://people.unica.it/brunmi/
Three PhD Positions in Multiscale Modeling and Experimental Characterization of Composites, Aluminum Alloys, and High Strength Steels
Applications are invited for three PhD positions within the Cognitive Performance Optimization Laboratory (COPOL) in the Department of Mechanical Engineering at the University of New Brunswick.
Open Stanford faculty position in Mechanical Engineering
The Department of Mechanical Engineering at Stanford University (http://me.stanford.edu/) invites applications for a tenure-track faculty appointment at the junior level (Assistant or untenured Associate Professor). Applications will be reviewed across all disciplines of mechanical engineering. As part of recent strategic planning, the department has identified special hiring needs and opportunities in controls, robotics, manufacturing, and biomedical engineering.
Two PhD positions are available immediately in Computational Materials & Mechanics
Two PhD positions are available immediately in the Computational Materials & Mechanics Laboratory at Missouri University of Science and Technology (Rolla), http://web.mst.edu/~aslezaeemm/.
The project is about multi-phase field modeling of formation and evolution of intermetallics and oxides at high temperatures.