Maximal energy that can be converted by a Dielectric Elastomer Generator
Mechanical energy can be converted to electrical energy by using a dielectric elastomer generator. The elastomer is susceptible to various modes of failure, including electrical breakdown, electromechanical instability, loss of tension, and rupture by stretch. The modes of failure define a cycle of maximal energy that can be converted. This cycle is represented on planes of work-conjugate coordinates, and may be used to guide the design of practical cycles.