Skip to main content

Going beyond 2D Neumann-Mullins (or, what is popularly known as, solving the beer froth structure)

Submitted by Mogadalai Gururajan on

Introduction

The blogosphere is abuzz with the latest report of the generalisation of the von Neumann-Mullins grain growth relation to 3 (and N) dimensions by MacPherson and Srolovitz (As an interesting aside, almost all the reports say mathematical structure of beer foam structure resolved, or words to that effect --hence, I also decided to join the bandwagon on that one). I heard Prof. Srolovitz describe the work in a seminar nearly six months ago. Based on my notes of the talk, I would like the explain their work in this post. Curvature in the following refers to mean curvature (and not Gaussian).

Microcantilever operated in liquid environment for in-vitro biomolecular detection

Submitted by Kilho Eom on

We have recently reported the piezoelectric thick film microcantilever, which enables the in-situ real-time detection of the protein related to disease (e.g. C reactive protein) in liquid environment. This work was published at APL (click here).

"In-situ real-time monitoring of biomolecular interactions based on resonating microcantilevers immersed in a viscous fluid"

Sample issue of Journal of Materials, a TMS publication

Submitted by Mogadalai Gururajan on

JOM is a monthly publication of TMS--The minerals, metals, and materials society. It covers a wide range of materials topics. I expecially like the overview articles, which, in four or five pages pack lots of information. Further, the historical articles about metallurgy and materials in ancient civilizations will interest those of you who like to read about history in general, and science history, in particular.

Chip-package interaction and interfacial delamination

Submitted by Zhen Zhang on

In flip-chip package, the mismatch of thermal expansion coefficients between the silicon die and packaging substrate induces concentrated stress field around the edges and corners of silicon die during assembly, testing and services. The concentrated stresses result in delamination on many interfaces on several levels of structures, in various length scales from tens of nanometers to hundreds of micrometers. A major challenge to model flip-chip packages is the huge variation of length scales, the complexity of microstructures, and diverse materials properties. In this paper, we simplify the structure to be silicon/substrate with wedge configuration, and neglect the small local features of integrated circuits. This macroscopic analysis on package level is generic with whatever small local features, as long as the physical processes of interest occur in the region where the concentrated stress field due to chip-packaging interaction dominates. Because it is the same driving force that motivates all of the flaws. Therefore, the different interface cracks with same size and same orientation but on different interfaces should have similar energy release rates provided that the cracks are much smaller than the macroscopic length. We calculate the energy release rate and the mode angle of crack on the chip-package interface based on the asymptotic linear elastic stress field. In a large range of crack length, the asymptotic solution agrees with finite element calculation very well. We discuss the simplified model and results in context of real applications. In addition, we find that the relation of energy release rate G and crack length a is not power-law since local mode mixity is dependent of crack length a. Therefore, the curve of G~a can be wavy and hardly goes to zero even if crack length a goes to atomically small. The local mode mixity plays an important role in crack behavior.

ICNM 2007

Submitted by zhan-sheng guo on

The International Conferences on Nonlinear Mechanics (ICNM-x) have been regarded as important series conferences in mechanics circles. The previous four meetings in the series were successfully held in Shanghai and Beijing in 1985, 1993, 1998 and 2002, respectively. In recent years, new achievements in this field have been made. Therefore, it is appropriate to organize a new conference on this vitally important area of applied mathematics and mechanics. The Fifth International Conference on Nonlinear Mechanics (ICNM-V) will be held in Shanghai. The Conference aims to provide an international forum for presenting the latest results and stimulating wider academic exchange for experts in the related fields all over the world.

In Memory of Professor Liviu Librescu

Submitted by Marek-Jerzy Pindera on

I had known Liviu since his early days in the Engineering Science and Mechanics Department at Virginia Tech when I was just beginning my own academic career. I had received my PhD from this department in 1981 in an area (composite materials) that at the time was at the cutting edge of high technology. In 1985 I had come back to VA Tech from the industry to continue working in this exciting area in which the ESM Department excelled world-wide. Liviu had arrived shortly thereafter with an already established reputation as a top-notch scientist.

Electromechanical hysteresis and coexistent states in dielectric elastomers

Submitted by Xuanhe Zhao on

Active polymers are being developed to mimic a salient feature of life: movement in response to stimuli. Large deformation can lead to intriguing phenomena; for example, recent experiments have shown that a voltage can deform a layer of a dielectric elastomer into two coexistent states, one being flat and the other wrinkled. This observation, as well as the needs to analyze large deformation under diverse stimuli, has led us to reexamine the theory of electromechanics.

Harder than diamond: Rhenium diboride

Submitted by Mogadalai Gururajan on

In the recent issue of Science, researchers from UCLA (Chung et al) report on an ambient pressure synthesis (using arc melting) of a compound, namely, rhenium diboride, which is superhard. Apparently, the material leaves scratch marks on the surface of diamond. Here is the abstract of the paper: