Effective Use of Focused Ion Beam (FIB) in Investigating Fundamental Mechanical Properties of Metals at the Sub-Micron Scale

Submitted by Julia R. Greer on

I would like to share some of our more recent findings on nano-pillar compression, namely the role of the surface treatment in plastic deformation at the nano-scale. Recent advances in the 2-beam focused ion beams technology (FIB) have enabled researchers to not only perform high-precision nanolithography and micro-machining, but also to apply these novel fabrication techniques to investigating a broad range of materials' properties at the sub-micron and nano-scales. In our work, the FIB is utilized in manufacturing of sub-micron cylinders, or nano-pillars, as well as of TEM cross-sections to directly investigate plasticity of metals at these small length scales. Single crystal nano-pillars, ranging in diameter between 300 nm and 870 nm, were fabricated in the FIB from epitaxial gold films on MgO substrates and subsequently compressed using a Nanoindenter fitted with a custom-fabricated diamond flat punch. We show convincingly that flow stresses strongly depend on the sample size, as some of our smaller specimens were found to plastically deform in uniaxial compression at stresses as high as 600 MPa, a value ~25 times higher than for bulk gold. We believe that these high strengths are hardened by dislocation starvation. In this mechanism, once the sample is small enough, the mobile dislocations have a higher probability of annihilating at a nearby free surface than of multiplying and being pinned by other dislocations. Contrary to this, if the dislocations are trapped inside the specimen by a coating, the strengthening mechanism is expected to be different. Here we present for the first time the comparison of plastic deformation of passivated and unpassivated single crystal specimens at the sub-micron scale. The role of free surfaces is investigated by comparing stress results of both as-FIB'd, annealed, and alumina-passivated pillars. Preliminary results show that ALD-coated pillars exhibit much higher flow stresses at equivalent sizes and strains compared with the uncoated samples. We also found that while FIB damage during pillar fabrication might account for a small portion of the strength increase, it is not the major contributor.

ASYMPTOTIC ELASTIC STRESS FIELDS AT SINGULAR POINTS

Submitted by Jim Barber on

Singular elastic stress fields are generally developed at sharp re-entrant corners and at the end of bonded interfaces between dissimilar elastic materials. This behaviour can present difficulties in both analytical and numerical solution of such problems. For example, excessive mesh refinement might be needed in a finite element solution.

Horacio Espinosa is awarded the 2007 SES Young Investigator Medal (Northwestern University)

Submitted by Yong Zhu on

Professor Horacio Espinosa at Northwestern University is awarded the 2007 Society of Engineering Sciences (SES) Young Investigator Medal in recognition of his outstanding work in the field of Engineering Science and Nanomaterials. For more information on Professor Espinosa's research, please visit his group website.

A Theory of Anharmonic Lattice Statics for Analysis of Defective Crystals

Submitted by arash_yavari on

This paper develops a theory of anharmonic lattice statics for the analysis of defective complex lattices. This theory differs from the classical treatments of defects in lattice statics in that it does not rely on harmonic and homogeneous force constants. Instead, it starts with an interatomic potential, possibly with in¯nite range as appropriate for situations with electrostatics, and calculates the equilibrium states of defects. In particular, the present theory accounts for the differences in the force constants near defects and in the bulk. The present formulation reduces the analysis of defective crystals to the solution of a system of nonlinear difference equations with appropriate boundary conditions. A harmonic problem is obtained by linearizing the nonlinear equations, and a method for obtaining analytical solutions is described in situations where one can exploit symmetry. It is then extended to the anharmonic problem using modified Newton-Raphson iteration. The method is demonstrated for model problems motivated by domain walls in ferroelectric materials.

Surface Roughness and Electrical Contact Resistance

Submitted by Jim Barber on

J.R.Barber

The contact of rough surfaces

Surfaces are rough on the microscopic scale, so contact is restricted to a few `actual contact areas'. If a current flows between two contacting bodies, it has to pass through these areas, causing an electrical contact resistance. The problem can be seen as analogous to a large number of people trying to get out of a hall through a small number of doors.

Classical treatments of the problem are mostly based on the approximation of the surfaces as a set of `asperities' of idealized shape. The real surfaces are represented as a statistical distribution of such asperities with height above some datum surface. However, modern measurement techniques have shown surfaces have multiscale, quasi-fractal characteristics over a wide range of length scales. This makes it difficult to decide on what scale to define the asperities.

A new finite element method for dislocations based on interior discontinuities

Submitted by Robert Gracie on

Comments and feedback of the following paper would be appreciated.

Abstract:

A new technique for the modelling of multiple dislocations based on introducing interior discontinuities is presented. In contrast to existing methods, the superposition of infinite domain solutions is avoided; interior discontinuities are specified on the dislocation slip surfaces and the resulting boundary value problem is solved by a finite element method. The accuracy of the proposed method is verified and its efficiency for multi-dislocation problems is illustrated. Bounded core energies are incorporated into the method through regularization of the discontinuities at their edges. Though the method is applied to edge dislocations here, its extension to other types of dislocations is straightforward.

New Directions in Large Deformation Solid Mechanics

Submitted by Luis Dorfmann on

We write to invite your participation in the symposium on New Directions in Large Deformation Solid Mechanics to be held at Texas A&M University campus in College Station as part of the 44th Annual Technical Meeting of the Society of Engineering Science, October 21–24, 2007. The purpose of this symposium is to address and outline new directions in large deformation solid mechanics and to furnish a forum for discussions on a wide range of research in all fields comprising modern mechanics.

Luis Dorfmann, Ray Ogden, Alan Wineman

5 PhD positions in solid mechanics

Submitted by tvpc22 on

There are 5 vacant PhD positions with good stipend in the field of solid mechanics, constitutive modelling and numerical simulations. We are looking for very competent, creative students all over the world. It is a rare opportunity for a young scientist to develop his versatile skills and this is your chance. As some people know, SIMLab (Structural Impact Laboratory) is internationally reputed group working on problems related to Crashworthiness and Structural Impact. Our group recently got a Centre for Research based Innovation (CRI). All these positions are filling under CRI. Please find the details in the links here:

Call for proposals on advanced high strength steel

Submitted by Ken P. Chong on

The Division of Civil, Mechanical and Manufacturing Innovation (CMMI) of NSF and the DOE Office of Freedom CAR and Vehicle Technologies intend to co-sponsor proposals addressing fundamental research issues in advanced high strength steels (AHSS). Specifically, proposals focused on

  1. AHSS materials development and characterization,
  2. predictive modeling that integrates AHSS material structure and product performance, and
  3. fundamental research in the area of processing and manufacturing of AHSS, are of interest. This collaborative effort is a direct outcome of the Advanced High Strength Steel Workshop.

Interested PIs should consider submitting an unsolicited proposal to the core programs of the CMMI Division namely, (1) Materials Processing & Manufacturing (MPM), (2) Materials Design & Surface Engineering (MDSE), (3) Applications & Structural Mechanics, or (4) Mechanics & Structures of Materials (MSM), during the January 15, 2007 to February 15, 2007 submission window. Unsolicited proposals in response to this letter should have titles beginning with "AHSS:".  Proposals from the March-April 2007 panel review will be eligible for co-funding, pending availability of funds.

J-Club participation: advice for students

Submitted by MichelleLOyen on
Choose a channel featured in the header of iMechanica

Now that the Journal Club is getting started, I wanted to post some advice for students who may not have participated in such a forum in the past, either online or in person. The fun of a J-club includes the opportunity to broaden your understanding of the literature of a broad field (like mechanics) by reading carefully-selected groups of papers on small topics of interest to different sub-communities. The challenge in participating in the subsequent discussion is ensuring that you understand the papers sufficiently to participate confidently in the ensuing discussion. This will also prepare you to be a good reviewer for technical journals some day.