Skip to main content

Research Assistant (PhD or Post Doc) in the field Mechanics of Adaptive Systems at Ruhr-Univesität Bochum, Germany

Submitted by AGMAS on

The Research Group Mechanics of Adaptive Systems at the Ruhr University Bochum (RUB) announces the available post for a

Research Assistant (PhD candidate or Post Doc)

with 39,83 working hours per week (work rate 100%), start date: as soon as possible, employment duration 3 years

Tasks:

Discussion of fracture paper #22 - Open access puts scientists in control of their own results

Submitted by ESIS on

The last ESIS blog about how surprisingly few scientists are willing/able to share their experimental data, received an unexpectedly large interest. Directly after the publication another iMechanica blogger took the same theme but he put the focus on results produced at numerical analyses that are presented with insufficient information. While reading, my spontaneous guess was that one obstacle to do right could be the widespread use of commercial non-open codes.

Call for Abstract Submission to SES2019 Symposium 3.9 Multiscale modeling of molecular, cellular, tissue, and organ mechanics

Submitted by Ying Li on

Dear Colleagues,

You are cordially invited to submit your one-page abstract to our Symposium 3.9 Multiscale modeling of molecular, cellular, tissue, and organ mechanics for The 56th Annual Technical Meeting of the Society of Engineering Science (SES2019) 

Date & Location:

Washington University in St. Louis (WashU) during 13-15 October 2019.

 

Directional and oscillating residual stress on the mesoscale in additively manufactured Ti-6Al-4V

Submitted by Mike Prime on

.
.

In this work, we were able to improve existing residual stress measurement capabilities so that we could measure smaller length scales. We were able to measure residual stresses that oscillated from build layer to build layer (0.5 mm thick) in an additively manufactured part. The oscillations persisted over nearly 30 layers!


The paper is free until April 20, 2019 at https://authors.elsevier.com/c/1YekJ4r9SUFESl

 

 

Call for abstracts: Symposium on 3D/4D printed functional materials and structures in 2019 SES Meeting

Submitted by Kai Yu on

Dear colleagues:

     We would like to invite you to submit an abstract to the symposium on 3D/4D printed functional materials and structures at the 2019 Society of Engineering Science meeting to be held from October 13 to October 15 on the campus of Washington University in St. Louis, MO, USA.

Urgent: 2 fully-funded PhD theses at Synopsis (Exeter) / Cardiff University / University of Luxembourg in machine learning/biomedical simulations/3D medical image processing

Submitted by Pierre Kerfriden on
Synopsys NE Ltd (https://www.synopsys.com/simpleware.html), Cardiff University and University of Luxembourg invites applications for 2 Early Stage Researcher position (Doctoral Candidate) as part of the Rapid Biomechanics and Simulation for Personalized Clinical Design (RAINBOW) MCSA European Training Network. RAINBOW is funded under the European Union’s Horizon 2020 research and innovation program.