Highly Stretchable and Sensitive Strain Sensor Based on Silver Nanowire–Elastomer Nanocomposite

Submitted by mortezaamjadi on

The demand for flexible and wearable electronic devices is increasing due to their facile interaction with human body. Flexible, stretchable and wearable sensors can be easily mounted on clothing or directly attached onto the body. Especially, highly stretchable and sensitive strain sensors are needed for the human motion detection. Here, we report highly flexible, stretchable and sensitive strain sensors based on the nanocomposite of silver nanowire (AgNW) network and PDMS elastomer in the form of the sandwich structure (i.e., AgNW thin film embedded between two layers of PDMS).

PhD position in the area of mechanics of energy storage materials at NJIT

Submitted by Siva P V Nadimpalli on

Hello,

There is an opening for a PhD student position in Dr. Nadimpalli’s group at the New Jersey Institute of Technology starting from Fall2015. Candidates with good academic credentials and an interest to work in experimental research projects are encouraged to apply. Ideal candidate should have a master’s degree in mechanical/materials science/aerospace or related field with a good background in Solid Mechanics, Materials Science, and Experimental Methods (including but not limited to SEM, TEM, and nanofabrication methods).

Call for abstracts for session "Mechanical Characterization of Soft Materials" in SES symposia 2015 at TAMU

Submitted by Yuhang Hu on

Symposium Title: “Mechanical Characterization of Soft Materials”

Organizers: Shengqiang Cai (shqcai [at] ucsd.edu) & Yuhang Hu (yuhanghu [at] illinois.edu)

Sessions: 2

Abstract:

Marie Curie Post-Doc position in Computational Thermomechanics at VESUVIUS (Belgium): deadline May 30, 2015

Submitted by ssmg-unitn-italy on

You will be hired for a 24 months assignment starting as soon as possible by

Vesuvius Company (Belgium) on a FP7 Marie Curie-IAPP project, in cooperation with

a very active group in Solid Mechanics at University of Trento.

 

The candidate will implement the constitutive models developed for high- temperature behaviour

of materials in external routines for finite elements computations and tested to judge the

numerical stability and accuracy. The software will be subsequently employed in the design

PhD Position in Experimental Mechanics at Extreme Temperatures

Submitted by ryanberke on

The Mechanics at Extreme Temperatures Lab at Utah State University is looking for qualified research assistants at the PhD level for Fall 2015. Research will be focused on mechanical characterization of two materials for advanced aerospace applications:

1. Molybdenum-base superalloys for advanced propulsion systems, and
2. Ultra-high temperature ceramics for the leading edges of spacecraft and hypersonic aircraft.

Marie Curie PhD position at University of Trento (Italy): deadline May 14, 2015

Submitted by ssmg-unitn-italy on

If you are strongly motivated to work with a very active group in Solid Mechanics,

we have a PhD position (3 years) available from June 2015,

but the deadline for application is May 14, 2015!

The position is on a EU grant and is addressed to numerical/theoretical modelling of ceramics.

For details on the application see the attachment.