Flexoelectricity in Bones: A nanophenomenon that triggers the bone-repair process

Submitted by Amir Abdollahi on

Bones generate electricity under pressure, and this electromechanical behavior is thought to be essential for bone's self-repair and remodeling properties. The origin of this response is attributed to the piezoelectricity of collagen, which is the main structural protein of bones. In theory, however, any material can also generate voltages in response to strain gradients, thanks to the property known as flexoelectricity.

Mechanical Reading of Ferroelectric Polarization

Submitted by Amir Abdollahi on

The mechanical properties of materials are insensitive to space inversion, even when they are crystallographically asymmetric. In practice, this means that turning a piezoelectric crystal upside down or switching the polarization of a ferroelectric should not change its mechanical response. Strain gradients, however, introduce an additional source of asymmetry that has mechanical consequences.

Fracture toughening and toughness asymmetry induced by flexoelectricity

Submitted by Amir Abdollahi on

Cracks generate the largest strain gradients that any material can withstand. Flexoelectricity (coupling between strain gradient and polarization) must therefore play an important role in fracture physics. Here we use a self-consistent continuum model to evidence two consequences of flexoelectricity in fracture: the resistance to fracture increases as structural size decreases, and it becomes asymmetric with respect to the sign of polarization. The latter phenomenon manifests itself in a range of intermediate sizes where piezo- and flexoelectricity compete.

Constructive and Destructive Interplay between Piezoelectricity and Flexoelectricity in Flexural Sensors and Actuators

Submitted by Amir Abdollahi on

Flexoelectricity is an electromechanical effect coupling polarization to strain gradients. It fundamentally differs from piezoelectricity because of its size-dependence and symmetry. Flexoelectricity is generally perceived as a small effect noticeable only at the nanoscale. Since ferroelectric ceramics have a particularly high flexoelectric coefficient, however, it may play a significant role as piezoelectric transducers shrink to the sub-micrometer scale. We examine this issue with a continuum model self-consistently treating piezo- and flexoelectricity.

Revisiting pyramid compression to quantify flexoelectricity: A three-dimensional simulation study

Submitted by Amir Abdollahi on

Flexoelectricity is a universal property of all dielectrics by which they generate a voltage in response to an inhomogeneous deformation. One of the controversial issues in this field concerns the magnitude of flexoelectric coefficients measured experimentally, which greatly exceed theoretical estimates. Furthermore, there is a broad scatter amongst experimental measurements. The truncated pyramid compression method is one of the common setups to quantify flexoelectricity, the interpretation of which relies on simplified analytical equations to estimate strain gradients.

A computational study of flexoelectricity

Submitted by Amir Abdollahi on

Flexoelectricity is a size-dependent electromechanical mechanism coupling polarization and strain gradient. It exists in a wide variety of materials, and is most noticeable for nanoscale objects, where strain gradients are higher. Simulations are important to understand flexoelectricity because experiments at very small scales are difficult, and analytical solutions are scarce. Here, we computationally evaluate the role of flexoelectricity in the electromechanical response of linear dielectric solids in two-dimensions.