Three-dimensional simulation of crack propagation in ferroelectric polycrystals: Effect of combined toughening mechanisms

Submitted by Amir Abdollahi on

We simulate the fracture processes of ferroelectric polycrystals in
three dimensions using a phase-field model. In this model, the grain
boundaries, cracks and ferroelectric domain walls are represented in a
diffuse way by three phase-fields. We thereby avoid the difficulty of
tracking the interfaces in three dimensions. The resulting model can
capture complex interactions between the crack and the polycrystalline
and ferroelectric domain  microstructures. The simulation results show
the effect of the microstructures on the fracture response of the
material. Crack deflection, crack bridging, crack branching and
ferroelastic domain switching are observed to act as the main fracture
toughening mechanisms in ferroelectric polycrystals. Our fully 3-D

Conducting crack propagation driven by electric fields in ferroelectric ceramics

Submitted by Amir Abdollahi on

This is a recent article in Acta Materialia on the propagation of conducting cracks in ferroelectric ceramics

Title: Conducting crack propagation driven by electric fields in ferroelectric ceramics

Authors: Amir Abdollahi and Irene Arias, Universitat Politecnica de Catalunya (UPC), Barcelona

Abstract:

Phase-field modeling of crack propagation in piezoelectric and ferroelectric materials

Submitted by Amir Abdollahi on

This is an accepted manuscript in Journal of the Mechanics and Physics of Solids

Title: Phase-field modeling of crack propagation in piezoelectric and ferroelectric materials with different electromechanical crack conditions

Authors: Amir Abdollahi and Irene Arias, Universitat Politecnica de Catalunya (UPC), Barcelona

 

Abstract:

Crack initiation patterns at electrode edges in multilayer ferroelectric actuators

Submitted by Amir Abdollahi on

This is the preprint of an article that will appear in Smart Materials and Structures (SMS)

Title: Crack initiation patterns at electrode edges in multilayer ferroelectric actuators

Authors: Amir Abdollahi and Irene Arias, Universitat Politecnica de Catalunya (UPC), Barcelona

 

Abstract:

Numerical simulation of intergranular and transgranular crack propagation in ferroelectric polycrystals

Submitted by Amir Abdollahi on

This is the preprint of an article that will appear in International Journal of Fracture (IJF)

Title: Numerical simulation of intergranular and transgranular crack propagation in ferroelectric polycrystals

Authors: Amir Abdollahi and Irene Arias, Universitat Politecnica de Catalunya (UPC), Barcelona

 

 

Abstract:

Slow-Fast Crack Propagation in Ferroelectric Single Crystals

Submitted by Amir Abdollahi on

Dear Colleague,

 

I have uploaded a video which shows the simulation of Slow-Fast crack propagation in ferroelectric single crystals:

http://www.youtube.com/watch?v=6E7WSVOVAWM

 

For technical details, please refer to our recently published paper in Acta Materialia:

http://www.sciencedirect.com/science/article/pii/S1359645411001777

 

Best regards,

Phase-field simulation of anisotropic crack propagation in ferroelectric single crystals

Submitted by Amir Abdollahi on

This is the preprint of an article that will appear in Modelling and Simulation in Materials Science and Engineering (MSMSE)

Title: Phase-field simulation of anisotropic crack propagation in ferroelectric single crystals: effect of microstructure on the fracture process

Authors: Amir Abdollahi and Irene Arias, Universitat Politecnica de Catalunya (UPC), Barcelona

 

 

Abstract: