POLYMER MATRIX COMPOSITES REINFORCED BY CARBON NANOTUBES

Submitted by Henry Tan on

CONTINUUM MODELING OF INTERFACES IN POLYMER MATRIX COMPOSITES REINFORCED BY CARBON NANOTUBES

L. Y. JIANG, H. TAN, J. WU, Y. HUANG, K. -C. HWANG
Review Article, 2007, accepted by NANO

The interface behavior may significantly influence the mechanical properties of carbon nanotube (CNT)-reinforced composites due to the large interface area per unit volume at the composite. The modeling of CNT/polymer interfaces has been a challenge in the continuum modeling of CNT reinforced composites.