New background of micromechanics of composites

Submitted by Valeriy Buryachenko on

Dear Colleagues,

One proposes a new background of micromechanics (NBM) of composites. NBM offers opportunities for a fundamental jump in multi-scale and multi-physics modeling of random heterogeneous media with drastically improved accuracy of local field estimations. In so doing, a difference of linear effective properties estimated by the use of either the new background or the classical one (proposed in 1830-1880) is not significant. See the abstract attached describing a list of 40 papers and conference presentations dedicated to the NBM.

 

A slip wave solution in anti-plane elasticity

Submitted by Ranjith Kunnath on

Abstract:

It is shown that a slip wave solution exists for anti-plane sliding of an elastic layer on an elastic half-space. It is a companion solution to the well-known Love wave solution.

https://dx.doi.org/10.1093/gji/ggw464

https://arxiv.org/abs/1612.01662

In Press, Geophysical Journal International, 2016

 

 

 

Society of Engineering Science - 2017 Medalists and Fellows

Submitted by Society of Eng… on

The Board of Directors of the Society of Engineering Science is pleased to announce the names of the 2017 Medalists and newly elected Fellows.

2017 SES Young Investigator Medals:

Oscar Lopez-Pamies (University of Illinois) for “Seminal contributions to the understanding of cavitation phenomena in rubber and the elastic dielectric behavior of filled elastomers by means of novel iterative homogenization techniques as well development of effective constitutive model for hyperelastic materials.

and

Postdoc Position in Mechanics of Polymer and Composite Materials Characterization

Submitted by Jie. Yin on

Applications are invited for an immediate postdoctoral associate opening in materials characterization at the Department of Mechanical Engineering, Temple University, Phiadelphia, PA. The project will focus on the mechanical property characterization of micro/nano-fibers and their woven structures for design of high energy absorption materials.

PhD/masters position in Mechanical Department at University of Hawaii at Manoa

Submitted by bardia on

A PhD/masters position is available in AMMI Lab at University of Hawaii at Manoa in the field of surgical robotics. Interested and outstanding candidates should visit my website at http://uhatmanoa.wixsite.com/ammi. Information about general admission process could be found on http://uhatmanoa.wixsite.com/ammi/prospective-students.

Damage modeling in Small Punch Test specimens

Submitted by Emilio Martíne… on

I hope some of you may find this work interesting:

Damage modeling in Small Punch Test specimens

E. Martínez-Pañeda, I.I. Cuesta, I. Peñuelas, A. Díaz, J.M. Alegre

Theoretical and Applied Fracture Mechanics, 86A, pp. 51-60

http://www.sciencedirect.com/science/article/pii/S0167844216301616