Blog posts
Force-driven evolution of mesoscale structure in engineered 3D microtissues and the modulation of tissue stiffening
Force-driven evolution of mesoscale structure in engineered 3D microtissues and the modulation of tissue stiffening
Ruogang Zhao, Christopher S. Chen, Daniel H. Reich, Biomaterials, Vol. 35, Issue 19, June 2014, Pg 5056–5064
http://www.sciencedirect.com/science/article/pii/S0142961214001604
Abstract:
MULTISCALE QUASICONTINUUM APPROACHES FOR DISCRETE MODELS OF FIBROUS MATERIALS SUCH AS ELECTRONIC TEXTILE AND PAPER MATERIALS
PhD studentship in Computational Medical Robotics - Strasbourg - Luxembourg - Cardiff
PhD studentship available http://icube-avr.unistra.fr/fr/index.php/Sujets_de_th%C3%A8ses#Simulati… http://icube-avr.unistra.fr/en/index.php/Open_Positions#PhD_Thesis_in_m…
Please contact Hadrien or myself for more details. Related recent publications:
TED University: Faculty Position in the Department of Mechanical Engineering, Ankara-Turkey
The Department of Mechanical Engineering (http://www.tedu.edu.tr/en-US/Content/Default.aspx) invites applications for a tenure track/tenured faculty position to begin September 2014.
For tenure track positions, highly motivated and research driven candidates are sought. For tenured faculty positions, the candidate should have demonstrated excellence in original research.
High order isogeometric cohesive elements for delamination analysis
Please find attached two recent papers on the use of high order B-splines/NURBS cohesive interface elements for an efficient modeling of delamination of composite laminates.
Mecahnics on the behaviour of Horizontal/laterally loaded thin hollow tubes
Dear all,
Please give some reading material on the horizontal/laterally loaded thin hollow tube, which explains with suitable formulas to calculate circumferential/hoop stresses in the thin tube subjected to lateral/horizontal loaḍ
visiting positions in Shanghai University
There are several visiting position openings in Shanghai University in the field of solid mechanics. Faculty members from domestic universities and foreign universities who are intereasted in the positions are welcome to contact with Professor Junqian Zhang (jqzhang2 [at] shu.edu.cn)
Contact modelling in Abaqus - Need urgent help
Dear all
I urgently need the answer to my question. I am modelling a clapping or contact between two surfaces similar to a crack.
I have used abaqus : 1-tangential : frictionless 2-Hard contact
I wanna know what moelling approach does abaqus use for above situation ?
Does abaqsu use hertzian contac ? bilinear stiffness or what ?
Thank you