Microstructural observations and tensile fracture behavior of FSW twin roll cast AZ31 Mg sheets

Submitted by a.dorbane on

Defect-free joints were friction stir welded (FSW) from AZ31 Mg alloy sheets by employing optimum welding parameters for the tool geometry used. Microstructure, texture and mechanical response of the welded joints were studied to identify susceptibility of crack initiation in the different weld zones and to understand the overall fracture behavior of these welds.

Observations of the mechanical response and evolution of damage of AA 6061-T6 under different strain rates and temperatures

Submitted by a.dorbane on

Investigated in this paper is the mechanical and microstructural response of specimens cut from rolled AA 6061-T6 alloy subjected to uniaxial loading at different temperatures (25, 100, 200, and 300 °C) and strain rates (10–4, 10−3, 10−2, 10−1 s−1). It was found that the material exhibits a strain rate and temperature dependent behavior. Microstructure observations reveal grains elongated in the loading direction with the average grain size being independent of loading conditions.

Facebook web-page of MUSAM online

Submitted by marco.paggi on

Dear Colleagues,

for those of you interested in being continuously updated on the activities of the Research Unit MUSAM on Multi-scale Analysis of Materials at the IMT School for Advanced Studies Lucca, research publications and open positions, please visit and join with your 'like' the new Facebook web page of MUSAM :

https://m.facebook.com/fanpagemusam

Thank you and best regards,

Marco Paggi 

Research Unit Director 

Two PhD positions at Department of Petroleum Engineering, Texas A&M University

Submitted by srabeedii on

Two PhD positions are available at Department of Petroleum Engineering, Texas A&M University in the area of characterization and micromechanical modeling of organic-rich shales. Candidates should have a BS or MS degree in  civil engineering, mechanical engineering, petroleum engineering, material science or other related areas. Candidates with both experimental and modeling background are highly preferred.

Two PhD positions at Department of Petroleum Engineering, Texas A&M University

Submitted by srabeedii on

Two PhD positions are available at Department of Petroleum Engineering, Texas A&M University in the area of characterization and micromechanical modeling of organic-rich shales. Candidates should have a BS or MS degree in  civil engineering, mechanical engineering, petroleum engineering, material science or other related areas. Candidates with both experimental and modeling background are highly preferred.

Structural simulation position @ Bosch

Submitted by Kadung on

Robert Bosch Engineering and Business Solutions is a branch of Robert Bosch (Fortune 500) is seeking a Senior Engineer for its Simulation team in Ho Chi Minh city, Vietnam. Only applicable for Vietnamese candidate or candidate can work in Vietnam

Senior structural simulation engineer

Requirements:

·         BSc, MSc or PhD in Mechanical Engineering, Computational Engineering, Maths or related fields

One Ph.D. student opening in the Department of Aerospace Engineering at the Iowa State University

Submitted by Shuozhi Xu on

The group of Prof. Liming Xiong at the Iowa State University has an immediate opening for a self-motivated Ph.D. student in the general area of computational solid mechanics and computational materials science. Atomistic simulation, DD, PFM and FEM experience will be a plus. The enrollment into the Ph.D. program is as early as Fall 2016, financially supported by a Research Assistantship. Please contact the PI directly if you are interested:

Experimental characterization of the heat transfer coefficient for hot stamping/ press hardening applications

Submitted by bitamendi on

Dear all, 

We just got published a new work titled " EXPERIMENTAL CHARACTERIZATION OF THE HEAT TRANSFER COEFFICIENT UNDER DIFFERENT CLOSE LOOP CONTROLLED PRESSURES AND DIE TEMPERATURES"