Dear All,I am studying cyclic loading, Plasticity and metal ratchetting. All the publication related to these topics mention about backstress. Please somebody explain me what is the backstress. Could you please suggest me a reference to learn fundamentals?bandula

 

Well, backstress, in my opinion, refers to the center of the yielding surface. For more information, you can read theory of plasticity, chap2.