Electric Field May Promote Exfoliation of Clay Nanoplates
Nanocomposite performance fundamentally relies on reproducible dispersion and arrangement of nanoparticles, such that the dominate morphology across macroscopic dimensions is also nanoscopic. To facilitate dispersion, chemical approaches, including surfactant or macromolecular stabilization are usually employed to modify the surface of nanoparticles. However, the approach depends on the material system and usually involves trial-and-error to identify the best practice. Much less quantitative information is available on the coupling between the surface modification and external processing factors, including shear, electric or magnetic fields. In a recent work, we considered electric field on the interaction of nano-plates. For ideal dielectrics an electric field may assist (or retard) exfoliation depending on the angle between a collection of plates and the field. A critical electric field strength to promote exfoliation is predicted when the field is parallel to the surface of the plates. Structural refinement is predicted to occur by cleavage through the center of the stack. For lossy dielectrics, frequency can be tuned to cause exfoliation in all plate orientations.
- Wei Lu's blog
- Log in or register to post comments
- 6758 reads
Comments
Can you insert a hyperlink in your post?
Your post sounds interesting. Can you insert a hyperlink into your post, pointing to a more complete description of this work?
You can also upload a file as an attachment to your post.