Influence of hydrogen functionalization on the fracture strength of graphene and the interfacial properties of graphene-polymer nanocomposite Submitted by Nuwan Dewapriya on Sat, 06/06/2015 - 16:07 research fracture of graphene interfacial adhesion molecular dynamics hydrogen functionalization strain rate temperature effects graphene hydrogen adatom graphene-polymer interface fracture toghness kinetic modelling Abstract Read more about Influence of hydrogen functionalization on the fracture strength of graphene and the interfacial properties of graphene-polymer nanocompositeLog in to post comments3445 views