Influence of hydrogen functionalization on the fracture strength of graphene and the interfacial properties of graphene–polymer nanocomposite. Submitted by Nuwan Dewapriya on Tue, 06/16/2015 - 05:45 research nano-fracture interfacial strength fracture of graphene molecular dynamics graphene-polymer interface Abstract Read more about Influence of hydrogen functionalization on the fracture strength of graphene and the interfacial properties of graphene–polymer nanocomposite.3 commentsLog in to post comments8766 views
Influence of hydrogen functionalization on the fracture strength of graphene and the interfacial properties of graphene-polymer nanocomposite Submitted by Nuwan Dewapriya on Sat, 06/06/2015 - 16:07 research fracture of graphene interfacial adhesion molecular dynamics hydrogen functionalization strain rate temperature effects graphene hydrogen adatom graphene-polymer interface fracture toghness kinetic modelling Abstract Read more about Influence of hydrogen functionalization on the fracture strength of graphene and the interfacial properties of graphene-polymer nanocompositeLog in to post comments3448 views