Influence of hydrogen functionalization on the fracture strength of graphene and the interfacial properties of graphene–polymer nanocomposite. Submitted by Nuwan Dewapriya on Tue, 06/16/2015 - 05:45 research nano-fracture interfacial strength fracture of graphene molecular dynamics graphene-polymer interface Abstract Read more about Influence of hydrogen functionalization on the fracture strength of graphene and the interfacial properties of graphene–polymer nanocomposite.3 commentsLog in to post comments8780 views